Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
PolyOne Maxxam™ MX5210-0040 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3433R PC 30% GR, provides improved mechanical properties. UV-stabilized. Internal mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Lubricomp RCP36XXP PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCP36XXP is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Lubricomp RCP36XXQ PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCP36XXQ is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 2410R PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP LX04015 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LX04015 is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include: Electrically Conductive |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm | 0.0020 - 0.0030 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics LNP Thermocomp RF0069 PA 66 (Europe-Africa-Middle East) Flame retarded, 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F102G30 PET, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL HFG300 PPE+PS (Asia Pacific) PPE+PS GF30% filled, FR V-0 |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB44S is a compound based on Polypropylene resin containing Glass Fiber, Glass Beads. Added features include; Heat Stabilized, Cu-Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RC004SXS is a compound based on PA 66 resin containing Carbon Fiber. Added features include; Heat Stabilized, Electrically Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL GFN3V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN3V is a 30 % glass fibre reinforced material with a HDT/A of 145C according ISO 75. NORYL GFN3V has been approved for potable water applications up to 85C by the UK WFBS according BS 6920 i.. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 4.00 mm |
0.0010 - 0.0030 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 4.00 mm |
0.0010 - 0.0030 in/in @Thickness 0.157 in |
E2P method |
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | on Tensile Bar; E2P method |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Clariant Renol PPOSP0001 Polyphenylene Oxide, Mineral Filled Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
Chase Plastics CP Pryme® PC330R Polycarbonate, 30% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Time 86400 sec |
0.0010 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |
|||
Linear Mold Shrinkage, Flow | 0.0010 - 0.0030 cm/cm @Thickness 3.20 mm |
0.0010 - 0.0030 in/in @Thickness 0.126 in |
ASTM D955 |
Samsung Cheil Industries Infino® XF-4150 PPA, Glass Filled Information provided by Samsung Cheil Industries. |