Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK/HF Post Consumer Recycle Nylon 6 Impact Modified, High Flow, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm @Thickness 3.17 mm |
0.015 - 0.019 in/in @Thickness 0.125 in |
ASTM D955 |
Ravago Manufacturing Americas Enviramid™ N2300THL BK Post Consumer Recycle Nylon 6 Impact Modified, Heat Stabilized, Lubricated, Black and Made from EnViramid Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
LyondellBasell Moplen HP400H Polypropylene Homopolymer Description: Moplen HP400H is a homopolymer for extrusion applications. Moplen HP400H exhibits easy processability and a good stiffness/impact balance at ambient temperature. The main applications .. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4, 2577 |
Kuraray Genestarâ„¢ N1001D-U03 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Time 86400 sec |
0.015 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing 20% Aramid. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.035 cm/cm @Time 86400 sec |
0.015 - 0.035 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP 0121 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.018 cm/cm @Thickness 3.20 mm |
0.015 - 0.018 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PP 0112 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 2.00 mm |
0.015 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P702J Polypropylene Injection Molding Key Characteristics:High clarityHigh stiffnessGood processabilityMicrowavable for cooking applicationsOdorlessSafe for food contactRecommended Applications:General purpose injection parts that requi.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | on Tensile Bar; ISO 294 |
Eurostar Staramide AST42K PA66, Impact Modified, Injection Molded AST42K is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ASTM D955 |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® CLR40 Thermoplastic Elastomer Elastocon® CLR40 is a transparent thermoplastic elastomer that has been developed for applications that require resilience, high strength properties and a good surface finish. Elastocon® CLR40 is.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.025 cm/cm | 0.015 - 0.025 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Eurotec |
Eurotec® Tecomid® NT40 NL PPA, unfilled, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | ISO 294-4 |
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade (PBT+X)-MD40Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | plate with film gate 150x150x3mm<sup>3</sup> |
BASF Ultradur® B 4560 PBT Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Sheet |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm | 0.015 in/in | Sheet |
BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.016 cm/cm | 0.015 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.17 mm |
0.015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
|
Unitika BV2120 PA66, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.019 cm/cm | 0.015 - 0.019 in/in | DIS 294-4 |
Wellman Wellamid® 42LH-WBK Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |