Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Nilit |
Nilit Polynil® C50L Externally Lubricated PA66/6 Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | Nilit |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.021 cm/cm | 0.013 - 0.021 in/in | ASTM D955 |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible B9000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294 |
Inno-Comp INNOPOL® CS 2-1000 Polypropylene Block-Copolymer INNOPOL® CS 2-1000 is a polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-1000 is developed for producing injection molded automo.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | 60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® TP 142-011 900116 Nylon 6 PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.0165 cm/cm | 0.013 - 0.0165 in/in | |
LATI Latistat 67-08 PA66, Impact Modified Dissipative product based on Polyamide 66 (PA66), impact modified. Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL0039XP PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RL0039XP is a compound based on PA66 resin containing PTFE, Flame Retardant. Added features include ; Flame Retardant, internally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WI001 is a compound based on Polybutylene Terephalate resin containing Silicone. Added features include; Inernally Lubricated. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 3.17 mm |
0.013 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6 FR-N IM Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Flame Retardant, Heat Stabilized, Impact Modified, Halogen Free and Lubricated Appearance: .. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Time 86400 sec |
0.013 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp PZ006 PA 6 (Asia Pacific) LNP* Thermocomp* PZ006 is a compound based on Nylon 6 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | 0.125 in; ASTM D955 |
Chase Plastics CP Pryme® NN300HL (Dry) Nylon 66, Heat Stabilized, Lubricated Features: General purposeHeat stabilizedLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® 42LN2-NBK2 Nylon 6, General Purpose All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | DIS 294-4 |
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 2800 J Polypropylene Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612
(Unverified Data**) Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.013 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
BASF Novolen® 2240 P Polypropylene Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
Polyplastic Armlen® PP MF 20-3-901 Polypropylene, 20% Mineral Filled Heat stabilized, low emission, black colorInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.013 cm/cm @Diameter 2.00 mm |
0.013 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, Conditioned Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |