| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded |
| Manufacturer | BASF |
| Trade Name | Novolen® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Novolen® 1148 TC Polypropylene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.910 g/cc | 0.0329 lb/in³ | |
| Water Absorption | 0.10 % | 0.10 % | |
| Moisture Absorption at Equilibrium | 0.10 % | 0.10 % | |
| Linear Mold Shrinkage, Flow | 0.013 cm/cm | 0.013 in/in | |
| Melt Flow | 72 g/10 min @Load 2.16 kg, Temperature 230 °C |
72 g/10 min @Load 4.76 lb, Temperature 446 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
| Elongation at Break | >= 50 % | >= 50 % | |
| Elongation at Yield | 9.0 % | 9.0 % | |
| Tensile Modulus | 1.55 GPa | 225 ksi | |
| Charpy Impact Unnotched | 10.3 J/cm² | 49.0 ft-lb/in² | |
| 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
||
| Charpy Impact, Notched | 0.200 J/cm² | 0.952 ft-lb/in² | |
| 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 135 µm/m-°C @Temperature 20.0 °C |
75.0 µin/in-°F @Temperature 68.0 °F |
|
| Melting Point | 163 °C | 325 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 95.0 °C | 203 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 57.0 °C | 135 °F | |
| Vicat Softening Point | 94.0 °C | 201 °F | |
| Flammability, UL94 | HB @Thickness 0.790 mm |
HB @Thickness 0.0311 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | |
| Dielectric Constant | 2.3 @Frequency 1e+6 Hz |
2.3 @Frequency 1e+6 Hz |
|
| Dielectric Strength | 140 kV/mm | 3560 kV/in | |
| Dissipation Factor | 0.00081 @Frequency 100 Hz |
0.00081 @Frequency 100 Hz |
|
| 0.0020 @Frequency 1e+6 Hz |
0.0020 @Frequency 1e+6 Hz |
||
| Comparative Tracking Index | 600 V | 600 V |