Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | 150x105x3; 300°C / MT 80°C; 400 bar; ISO 2577 |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | ISO 294-4, 2577 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | |
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good electrical properties.Availability: Africa &.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0050 cm/cm | 0.0035 - 0.0050 in/in | |
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latilub 66-10T G/30-V0KB1 PA66, 10% Glass Fiber Reinforced, PTFE Filled, Flame Retardant Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0060 cm/cm | 0.0035 - 0.0060 in/in | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latilub 82-05GR G/30 PA12, 30% Glass Fiber Reinforced, Graphite Filled Self-lubricating product based on Polyamide 12 (PA12). Graphite. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | |
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | SABIC Method |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® PC 04008 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF10 A1 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS LG GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerFeatures: Good UV Resistance and Low GlassAppearance: BlackInform.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® HDPE GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PA6/6 GF40 ML2 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0035 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PC GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.17 mm |
0.0035 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm @Thickness 3.00 mm |
0.0035 in/in @Thickness 0.118 in |
|
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0075 cm/cm | 0.0035 - 0.0075 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRGF1583-WT1 44% Mineral/Glass Reinforced Nylon 6 Description: Mineral/Glass Reinforced Nylon 6Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0035 cm/cm | 0.0035 in/in | Annealed; ISO 294-4 |
DuPont Performance Polymers Crastin® SK609 NC010 PBT
(Unverified Data**) Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | |
LATI Latiohm 66-10 H2 CNT G/35 PA66, 35% Glass Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Linear Mold Shrinkage, Flow | 0.0035 - 0.0065 cm/cm | 0.0035 - 0.0065 in/in | |
LATI Latimass 82-05 D040 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |