Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0080 - 0.018 cm/cm | 0.0080 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KG30 Nylon 6 for injection molding, 30% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.010 - 0.018 cm/cm | 0.010 - 0.018 in/in | FRISETTA Test Method |
Nilit FRIANYL B63 KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Linear Mold Shrinkage | 0.013 - 0.018 cm/cm | 0.013 - 0.018 in/in | ASTM D955 |
Polymer Resources PC/TP-GP3-IM PC/Polyester Alloy, Impact Modified Superior Chemical Resistance, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | after bake; ISO 294 |
Solvay Engineered Polymers DEXFLEX® 810HS TPO
(discontinued **) Description: DEXFLEX® 810HS is a thermoplastic olefinic elastomer (TPO) that offers excellent weatherability, paintability and processability. This material is designed to exceed the requirements .. |
|||
Linear Mold Shrinkage | 0.013 - 0.018 cm/cm | 0.013 - 0.018 in/in | ASTM D955 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Linear Mold Shrinkage | 0.011 - 0.018 cm/cm | 0.011 - 0.018 in/in | |
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm @Thickness 1.60 mm |
0.012 - 0.018 in/in @Thickness 0.0630 in |
ASTM D955 |
Gromax PBT 1100-211D Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm @Thickness 1.60 mm |
0.012 - 0.018 in/in @Thickness 0.0630 in |
ASTM D955 |
Gromax CCP PBT 1100-600S Product Description: PBT unreinforced high viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excell.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D955 |
Teknor Apex APEX® 7500-70 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm | 0.012 - 0.018 in/in | ASTM D955 |
Teknor Apex Chemlon® 100 W Nylon 66, Unreinforced Notes: MoS2 modified; Molybdenum disulphide modified to provide self-lubrication and low friction to parts subjected to wear and abrasion. FMVSS Flammability: Passes, FMVSS 302Processing Method: Inj.. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.018 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO DIS 294-4 |
Wellman Wellamid® FR22F-NBK3 Flame Retardant Nylon 66 Description: Flame Retardant Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm |
0.0060 - 0.018 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm |
0.0060 - 0.018 in/in @Thickness 0.126 in |
72 hr; ISO 294 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Linear Mold Shrinkage | 0.0060 - 0.018 cm/cm @Thickness 3.20 mm, Time 259000 sec |
0.0060 - 0.018 in/in @Thickness 0.126 in, Time 72.0 hour |
ISO 294 |
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo.. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | |
Polyram PlusTek RA102 Nylon 6.6, General Purpose General purpose polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO 2577 |
Polyram PlusTek RA115 Nylon 66 for Injection Molding Nylon 66 for injection molding applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.015 - 0.018 cm/cm | 0.015 - 0.018 in/in | ASTM D 955 |
Cossa Polimeri ESTAPROP 1000 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, PBDE free, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Linear Mold Shrinkage | 0.0080 - 0.018 cm/cm | 0.0080 - 0.018 in/in | ASTM D955 |
Buckeye Polymers BP FLEX D0850 BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Linear Mold Shrinkage | 0.012 - 0.018 cm/cm @Thickness 1.60 mm |
0.012 - 0.018 in/in @Thickness 0.0630 in |
ASTM D955 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |