Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
Manufacturer | Polyram |
Trade Name | PlusTek |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Polyram PlusTek RA115 Nylon 66 for Injection Molding.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 2.8 % | 2.8 % | 50% RH; ISO 62 |
Water Absorption at Saturation | 8.5 % | 8.5 % | ISO 62 |
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | ISO 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 118 | 118 | |
Tensile Strength, Yield | 85.0 MPa | 12300 psi | ISO 527 |
Elongation at Break | 25 % | 25 % | ISO 527 |
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Flexural Strength | 135 MPa | 19600 psi | ISO 178 |
Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
Izod Impact, Notched (ISO) | 4.50 kJ/m² | 2.14 ft-lb/in² | ISO 180 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 256 °C | 493 °F | ISO 11357 |
Maximum Service Temperature, Air | 70.0 °C | 158 °F | Continuous use |
100 °C | 212 °F | Short peaks operation | |
Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 100 °C | 212 °F | ISO 75 |
Glow Wire Test | 750 °C | 1380 °F | GWFI; IEC 60695 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Dielectric Constant | 3.6 @Frequency 1.00e+6 Hz |
3.6 @Frequency 1.00e+6 Hz |
IEC 60250 |
Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60250 |