Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYelast TPE R44 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | Across Flow; ISO 2577 |
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.013 - 0.020 cm/cm | 0.013 - 0.020 in/in | |
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Linear Mold Shrinkage | 0.013 - 0.015 cm/cm | 0.013 - 0.015 in/in | ASTM D955 |
Kolon KOPA® KN126 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Linear Mold Shrinkage | 0.013 - 0.016 cm/cm | 0.013 - 0.016 in/in | ASTM D955 |
Kolon KOPA® KN3322VO Flame Retardant Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 6006 GREY Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Multibase Multi-Flex® A 8502 LC UV RXF/YYWA Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2295 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Linear Mold Shrinkage | 0.013 - 0.017 cm/cm | 0.013 - 0.017 in/in | ISO 2577 |
Polyram PlusTek PA201 Nylon 66 for Extrusion High viscosity Nylon 66 for extrusion applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ±0.1 after 30 min.; ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010-01 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 1010-01 is an injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properties and flow characteristics .. |
|||
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
|
Toyobo PELPRENE™ S2002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 2.00 mm |
0.013 in/in @Thickness 0.0787 in |
|
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.013 cm/cm @Thickness 3.175 mm |
0.013 in/in @Thickness 0.1250 in |
ASTM D955 |
A. Schulman SCHULAMID® 66 MV3HI High Impact Nylon 6/6 Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
A. Schulman POLYFLAM™ E-15937B High Strength Impact Modified Polypropylene DescriptionPolyfort® E-15937B is a high strength impact modified polypropylene.Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ±0.1 after 30 min.; ASTM D1238 |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM Data; MD |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
Ashley Polymers Ashlene® 520MS/520SMS Nylon 66, MoS2 Filled A general purpose Molybdenum-disulfide filled nylon resin.Data provided by the manufacturer |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.013 - 0.020 cm/cm | 0.013 - 0.020 in/in | ASTM D955 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |