Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
Nylene® Naxel™ PC504 20% Glass Reinforced Polycarbonate Description: Naxel™ PC504 is a 20% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Network Polymers SAN 277 Blue Tint Color Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | With Flow; ISO 2577 |
Polykemi AB SCANAMID 66 A12^ F35 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | With Flow; ISO 2577 |
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Linear Mold Shrinkage | 0.0030 - 0.012 cm/cm | 0.0030 - 0.012 in/in | ASTM D955 |
Polymer Resources NY66-G60 Nylon 66, 60% Glass Reinforced Nylon 66, 60% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | 0.125 in, DAM; ASTM D955 |
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
PolyOne Lubri-Tech™ PS-30GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Kolon KOPET® KP132G30VO FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Samsung Cheil Industries Starex® SD-0150GP High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | ASTM D955 |
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | |
Polyram PlusTek PA303G33 Nylon 6.6, 33% Glass Fiber 33% glass fiber reinforced, heat stabilized and hydrolysis resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ISO 2577 |
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction 30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
Toyobo Vylopet® EMC130-01 Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: General and high rigidity componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric stren.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm @Thickness 1.59 mm |
0.0030 in/in @Thickness 0.0625 in |
ASTM D955 |
Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuou.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
Eastman Eastar AN014 Copolyester Eastar AN014 copolyester is a high flow product that contains a mold release. Eastar AN014 flow lengths are increased 20-40% relative to Eastar AN004 as shown by spiral flow testing. Other outstandi.. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D955 |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Linear Mold Shrinkage | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | ASTM D955 |
Diamond Polymers ASA TW-15H Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat Resistance, High IzodInformation provided by Diamond Polymers, Inc. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | |
E-Polymers TEKASTER® F10G30FR 30% Glass Fiber Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | MD; ASTM D955 |
Aclo Accutech Polypropylene Homopolymer HP0336G15M15CL Glass/Mineral Reinforced Coupled |
|||
Linear Mold Shrinkage | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D-955 |
Bhansali Engineering Abstron KU-650M ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D-955 |
Axiall 2651 Rigid PVC, Molding Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Linear Mold Shrinkage | 0.0030 - 0.0035 cm/cm | 0.0030 - 0.0035 in/in | ASTM D955 |
PolyOne Edgetek® UR-20CF/000 Thermoplastic Elastomer - TPU, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |