Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.58 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.14 - 1.58 g/cc
0.0412 - 0.0571 lb/in³
Average value: 1.42 g/cc Grade Count:7
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Density 1.20 - 1.58 g/cc
0.0434 - 0.0571 lb/in³
Average value: 1.47 g/cc Grade Count:47
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Density 1.07 - 1.58 g/cc
0.0387 - 0.0571 lb/in³
Average value: 1.22 g/cc Grade Count:22
Overview of materials for ABS/Polyester Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat..
Density 1.20 - 1.58 g/cc
0.0434 - 0.0571 lb/in³
Average value: 1.37 g/cc Grade Count:21
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Density 1.40 - 1.58 g/cc
0.0506 - 0.0571 lb/in³
Average value: 1.48 g/cc Grade Count:7
Overview of materials for Polyamide-Imide, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp..
Density 1.46 - 1.58 g/cc
0.0527 - 0.0571 lb/in³
Average value: 1.50 g/cc Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum ..
Density 1.30 - 1.58 g/cc
0.0470 - 0.0571 lb/in³
Average value: 1.46 g/cc Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Density 1.43 - 1.58 g/cc
0.0517 - 0.0571 lb/in³
Average value: 1.49 g/cc Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Density 1.18 - 1.58 g/cc
0.0426 - 0.0571 lb/in³
Average value: 1.35 g/cc Grade Count:14
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1184
Fainplast Compounds RE 325/2 Rigid PVC, Extrusion
Building profiles
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1184
Fainplast Compounds RE 625 Rigid PVC, Extrusion
Spiral pipes
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1184
Fainplast Compounds RE 925 Rigid PVC, Extrusion
Various profiles
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Fainplast Compounds AP 80 Flexible PVC, Flame Retardant Insulation
General purposes
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Fainplast Compounds GA 77/1 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Fainplast Compounds GA 89 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.27 - 1.58 g/cc
0.0459 - 0.0571 lb/in³
Average value: 1.40 g/cc Grade Count:32
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi..
Copyright © lookpolymers.com All Rights Reserved