Material Notes:
General purposes
Physical Properties Metric English Comments
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82
78 - 82
ISO R 868
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ISO R 527
Elongation at Break >= 260 %
>= 260 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm

@Temperature 23.0 °C
1.00e+13 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 75
CEI 20-34/3-2