Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D223 GF10 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183/A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66 LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXQ PPA LNP* LUBRICOMP* UFL36SXQ is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15%PTFE. Added features of this material include: Wear Resistant, Heat Stabilized, Bearing Grade. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Techmer ES HiFill® HTN GF HS L High Temp Nylon 50% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Heat ResistanceInformation provided by TP Composit.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hGR30 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp PF00A PA 6 (Europe-Africa-Middle East) 50% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66 LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM F1315 |
Thermoseal KLINGERSIL® C-4430 Compressed Inorganic Fiber Gasketing Synthetic FiberNitrile BinderExcellent Steam SheetExcellent Chemical ResistanceGood Creep RelaxationGeneral Purpose SheetInformation provided by Thermoseal Inc. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
Hexcel® HexMC™ C / 2000 / R1 Composite SMC High performance sheet-molding compound, specifically designed for compression molding. The epoxy matrix and high carbon fiber volume enable components to be molded for a wide range of applications.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40 Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Barlog Plastics KEBAFORM C 904 GB POM Copolymer, 20% glass bead reinforced POM-GB20Information provided by BARLOG plastics GmbH. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
BASF Petra® 7030 GY6128 30% Glass Filled PET Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® E126 PET Polyester, 30% Glass Reinforced PET Polyester, economy grade with 30% glass reinforcement.Data provided by the manufacturer |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | |
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
Lanxess Pocan® B 3235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
DSM Arnite® TV4 460 KL PBT/PET Blend-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
LNP Lubricomp® PDX-O-97635 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **)&l Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Density | 1.55 g/cc | 0.0560 lb/in³ | ISO 1183 |
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |