| Category | Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced | 
| Manufacturer | Ashley Polymers | 
| Trade Name | Ashlene® | 
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Ashley Polymers Ashlene® E126 PET Polyester, 30% Glass Reinforced.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.55 g/cc | 0.0560 lb/in³ | ASTM D792 | 
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 | 
| Tensile Strength, Yield | 135 MPa | 19600 psi | ASTM D638 | 
| Elongation at Break | 2.2 % | 2.2 % | |
| Flexural Strength | 207 MPa | 30000 psi | ASTM D790 | 
| Flexural Modulus | 7.60 GPa | 1100 ksi | ASTM D790 | 
| Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 245 °C | 473 °F | ASTM D3418 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | ASTM D648 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Dielectric Constant | 3.5 @Frequency 1e+6 Hz | 3.5 @Frequency 1e+6 Hz | ASTM D150 | 
| Dielectric Strength | 22.0           kV/mm @Thickness 3.20 mm | 559           kV/in @Thickness 0.126 in | Short Time; ASTM D149 | 
| Dissipation Factor | 0.021 @Frequency 1e+6 Hz | 0.021 @Frequency 1e+6 Hz | ASTM D150 |