A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 195 MPa
28300 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 319 MPa
46300 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 268 °C
514 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 271 - 285 °C
520 - 545 °F