Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-1 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-2 Linear Low Density Polyethylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-3 Polyethylene, 65% Mineral Filled 50% Calcium Carbonate / 15% Titanium Oxide FilledInformation provided by PolyPlastic Group. |
|||
Density | 1.64 - 1.65 g/cc | 0.0592 - 0.0596 lb/in³ | ISO 1183 |
Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate Information provided by PolyPlastic Group. |
|||
Density | 1.20 - 1.65 g/cc | 0.0434 - 0.0596 lb/in³ | Average value: 1.37 g/cc Grade Count:52 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.26 - 1.65 g/cc | 0.0454 - 0.0596 lb/in³ | Average value: 1.33 g/cc Grade Count:74 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.37 - 1.65 g/cc | 0.0495 - 0.0596 lb/in³ | Average value: 1.53 g/cc Grade Count:11 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Density | 1.39 - 1.65 g/cc | 0.0502 - 0.0596 lb/in³ | Average value: 1.52 g/cc Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Density | 1.15 - 1.65 g/cc | 0.0415 - 0.0596 lb/in³ | Average value: 1.33 g/cc Grade Count:36 |
Overview of materials for PVC, Sheet Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Sheet Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.549 - 1.65 g/cc | 0.0198 - 0.0596 lb/in³ | Average value: 1.31 g/cc Grade Count:408 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.08 - 1.65 g/cc | 0.0390 - 0.0596 lb/in³ | Average value: 1.32 g/cc Grade Count:14 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Density | 1.11 - 1.65 g/cc | 0.0401 - 0.0596 lb/in³ | Average value: 1.21 g/cc Grade Count:22 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Density | 1.61 - 1.65 g/cc | 0.0582 - 0.0596 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 337 Rigid PVC, Extrusion Cheap profiles |
|||
Density | 1.50 - 1.65 g/cc | 0.0542 - 0.0596 lb/in³ | |
Goodfellow Carbon/Vinyl Ester Rod Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Density | 1.50 - 1.65 g/cc | 0.0542 - 0.0596 lb/in³ | |
Goodfellow Carbon/Vinyl Ester Tube Carbon Fiber - Vinyl ester MatrixInformation provided by Goodfellow. |
|||
Density | 1.60 - 1.65 g/cc | 0.0578 - 0.0596 lb/in³ | |
Chengdu Polyster RPM450 Flame Retardant Masterbatch RPM 450 is a red phosphorus based additive flame retardant designed for uses in both glass-fiber reinforced and no-GF reinforced polyamides resins. It is halogen-free and shows more effective flame.. |
|||
Density | 1.22 - 1.65 g/cc | 0.0441 - 0.0596 lb/in³ | Average value: 1.43 g/cc Grade Count:37 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.33 - 1.65 g/cc | 0.0480 - 0.0596 lb/in³ | Average value: 1.48 g/cc Grade Count:25 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.26 - 1.65 g/cc | 0.0455 - 0.0596 lb/in³ | Average value: 1.48 g/cc Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Density | 1.33 - 1.65 g/cc | 0.0480 - 0.0596 lb/in³ | Average value: 1.42 g/cc Grade Count:31 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |
|||
Density | 1.34 - 1.65 g/cc | 0.0484 - 0.0596 lb/in³ | Average value: 1.40 g/cc Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Density | 1.61 - 1.65 g/cc | 0.0582 - 0.0596 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 9030 Flexible PVC, Lead Free Various profiles |