Fainplast Compounds RE 337 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Fainplast Compounds RE 337 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cheap profiles
Physical Properties Metric English Comments
Density 1.61 - 1.65 g/cc
0.0582 - 0.0596 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ISO R 527
Tensile Strength, Yield 34.0 MPa
4930 psi
ISO R527
Elongation at Break 80 %
80 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 - 81.0 °C

@Load 5.00 kg
174 - 178 °F

@Load 11.0 lb
ISO R306