| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Overview of materials for PVC, Rigid Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.549 - 1.65 g/cc | 0.0198 - 0.0596 lb/in³ | Average value: 1.31 g/cc Grade Count:408 |
| Filler Content | 10.0 - 20.0 % | 10.0 - 20.0 % | Average value: 15.0 % Grade Count:4 |
| Volatile Organic Compounds (VOC) Content | 0.300 - 0.500 g/l | 0.300 - 0.500 g/l | Average value: 0.314 g/l Grade Count:14 |
| Apparent Bulk Density | 0.550 - 0.650 g/cc | 0.0199 - 0.0235 lb/in³ | Average value: 0.576 g/cc Grade Count:17 |
| Particle Size | 63.0 - 250 µm | 63.0 - 250 µm | Average value: 155 µm Grade Count:14 |
| Viscosity Test | 61.0 - 116 cm³/g | 61.0 - 116 cm³/g | Average value: 96.0 cm³/g Grade Count:15 |
| Linear Mold Shrinkage | 0.000500 - 0.0120 cm/cm | 0.000500 - 0.0120 in/in | Average value: 0.00394 cm/cm Grade Count:76 |
| Melt Flow | 3.50 - 54.0 g/10 min | 3.50 - 54.0 g/10 min | Average value: 22.6 g/10 min Grade Count:4 |
| Spiral Flow | 53.3 - 119 cm | 21.0 - 47.0 in | Average value: 79.0 cm Grade Count:62 |
| ASTM Color | -15.8 - 81.0 | -15.8 - 81.0 | Average value: 17.5 Grade Count:4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 100 - 111 | 100 - 111 | Average value: 104 Grade Count:24 |
| Hardness, Shore D | 47.0 - 88.0 | 47.0 - 88.0 | Average value: 80.2 Grade Count:329 |
| Hardness, Shore C | 69.0 - 90.0 | 69.0 - 90.0 | Average value: 80.4 Grade Count:7 |
| Tensile Strength, Ultimate | 14.3 - 50.3 MPa | 2080 - 7300 psi | Average value: 38.0 MPa Grade Count:56 |
| Tensile Strength, Yield | 14.8 - 103 MPa | 2150 - 14900 psi | Average value: 46.3 MPa Grade Count:363 |
| Elongation at Break | 2.00 - 330 % | 2.00 - 330 % | Average value: 93.3 % Grade Count:143 |
| Elongation at Yield | 3.10 - 6.00 % | 3.10 - 6.00 % | Average value: 5.07 % Grade Count:6 |
| Modulus of Elasticity | 1.06 - 9.65 GPa | 154 - 1400 ksi | Average value: 2.83 GPa Grade Count:311 |
| Flexural Yield Strength | 29.1 - 159 MPa | 4220 - 23100 psi | Average value: 81.1 MPa Grade Count:304 |
| Flexural Modulus | 0.220 - 9.31 GPa | 31.9 - 1350 ksi | Average value: 2.85 GPa Grade Count:307 |
| Poissons Ratio | 0.400 - 0.440 | 0.400 - 0.440 | Average value: 0.420 Grade Count:9 |
| Shear Modulus | 1.44 - 3.45 GPa | 209 - 500 ksi | Average value: 2.28 GPa Grade Count:9 |
| Izod Impact, Notched | 0.160 - 14.0 J/cm | 0.300 - 26.2 ft-lb/in | Average value: 4.85 J/cm Grade Count:355 |
| 5.30 - 5.30 J/cm <br>@Temperature -10.0 - -10.0 °C |
9.93 - 9.93 ft-lb/in <br>@Temperature 14.0 - 14.0 °F |
Average value: 2.37 J/cm Grade Count:1 | |
| 0.267 - 11.7 J/cm <br>@Temperature -40.0 - 10.0 °C |
0.500 - 21.9 ft-lb/in <br>@Temperature -40.0 - 50.0 °F |
Average value: 2.37 J/cm Grade Count:56 | |
| 0.267 - 11.7 J/cm <br>@Thickness 3.18 - 3.18 mm |
0.500 - 21.9 ft-lb/in <br>@Thickness 0.125 - 0.125 in |
Average value: 2.37 J/cm Grade Count:56 | |
| Izod Impact, Unnotched | 0.392 - 9.70 J/cm | 0.735 - 18.2 ft-lb/in | Average value: 3.74 J/cm Grade Count:22 |
| Charpy Impact Unnotched | NB | NB | Grade Count:5 |
| Charpy Impact, Notched | 0.250 - 1.10 J/cm² | 1.19 - 5.24 ft-lb/in² | Average value: 0.582 J/cm² Grade Count:4 |
| Dart Drop, Total Energy | 19.8 - 21.9 J <br>@Temperature -18.0 - 0.000 °C |
14.6 - 16.2 ft-lb <br>@Temperature -0.400 - 32.0 °F |
Average value: 20.8 J Grade Count:1 |
| 19.8 - 21.9 J <br>@Thickness 1.85 - 1.85 mm |
14.6 - 16.2 ft-lb <br>@Thickness 0.0728 - 0.0728 in |
Average value: 20.8 J Grade Count:1 | |
| Dart Drop Total Energy | 5.34 - 280 J/cm | 0.0100 - 0.525 ft-lb/mil | Average value: 91.9 J/cm Grade Count:160 |
| 40.0 - 66.7 J/cm <br>@Temperature 0.000 - 0.000 °C |
0.0749 - 0.125 ft-lb/mil <br>@Temperature 32.0 - 32.0 °F |
Average value: 46.4 J/cm Grade Count:4 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 18.0 - 140 µm/m-°C | 10.0 - 77.8 µin/in-°F | Average value: 63.7 µm/m-°C Grade Count:163 |
| Maximum Service Temperature, Air | 60.0 - 190 °C | 140 - 374 °F | Average value: 167 °C Grade Count:35 |
| Deflection Temperature at 0.46 MPa (66 psi) | 41.1 - 88.9 °C | 106 - 192 °F | Average value: 72.5 °C Grade Count:81 |
| Deflection Temperature at 1.8 MPa (264 psi) | 17.8 - 86.1 °C | 64.0 - 187 °F | Average value: 68.3 °C Grade Count:310 |
| Vicat Softening Point | 51.0 - 97.8 °C | 124 - 208 °F | Average value: 81.7 °C Grade Count:67 |
| Brittleness Temperature | -30.0 - 15.0 °C | -22.0 - 59.0 °F | Average value: -13.1 °C Grade Count:8 |
| UL RTI, Electrical | 29.4 - 90.0 °C | 84.9 - 194 °F | Average value: 71.2 °C Grade Count:40 |
| 105 - 105 °C <br>@Temperature 105 - 105 °C |
221 - 221 °F <br>@Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 | |
| UL RTI, Mechanical with Impact | 10.0 - 85.0 °C | 50.0 - 185 °F | Average value: 59.7 °C Grade Count:35 |
| 105 - 105 °C <br>@Temperature 105 - 105 °C |
221 - 221 °F <br>@Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 | |
| UL RTI, Mechanical without Impact | 29.4 - 90.0 °C | 84.9 - 194 °F | Average value: 70.2 °C Grade Count:40 |
| 105 - 105 °C <br>@Temperature 105 - 105 °C |
221 - 221 °F <br>@Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 | |
| Flammability, UL94 | HB - 5VA | HB - 5VA | Grade Count:108 |
| Oxygen Index | 24.0 - 52.0 % | 24.0 - 52.0 % | Average value: 31.8 % Grade Count:10 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 4.00 - 8.00 % | 4.00 - 8.00 % | Average value: 5.10 % Grade Count:10 |
| Gloss | 5.00 - 60.0 % | 5.00 - 60.0 % | Average value: 28.1 % Grade Count:4 |
| Transmission, Visible | 7.50 - 90.0 % | 7.50 - 90.0 % | Average value: 78.3 % Grade Count:51 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dissipation Factor | 0.0290 - 0.0400 <br>@Temperature 30.0 - 30.0 °C |
0.0290 - 0.0400 <br>@Temperature 86.0 - 86.0 °F |
Average value: 0.0345 Grade Count:1 |
| 0.0290 - 0.0400 <br>@Frequency 60.0 - 1000 Hz |
0.0290 - 0.0400 <br>@Frequency 60.0 - 1000 Hz |
Average value: 0.0345 Grade Count:1 | |
| Comparative Tracking Index | 600 V | 600 V | Average value: 600 V Grade Count:5 |
| Hot Wire Ignition, HWI | 60.0 - 120 sec | 60.0 - 120 sec | Average value: 90.0 sec Grade Count:5 |
| High Amp Arc Ignition, HAI | 60.0 - 120 arcs | 60.0 - 120 arcs | Average value: 90.0 arcs Grade Count:5 |