Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7020X X-Ply Cross-Ply Polyethylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IS7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous S-Glass (ThermoPro-S™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement
(discontinu Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperatu.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Aremco Aremco-Bond™ 597 Conductive Epoxy Adhesive
(discontinued **) Electrically and thermally conductive, silver-filled, one-part paste. Inorganic system for adhesive (597A) & coating (597C) applications to 1200 ºF (650 °C). |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® K-FHG12 (Cond.) 60% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Density | 1.66 - 1.92 g/cc | 0.0600 - 0.0694 lb/in³ | Average value: 1.77 g/cc Grade Count:15 |
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D572 |
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
LATI Latilub 85-10T G/30 PES, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyether Sulfone (PES). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-4-240NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-240NA and R-4-240BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and toughness compared to other polyphenylene sulfide compounds.Feat.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp JF008 PES LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT (Asia Pacific) LNP* THERMOCOMP* WF008 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON UV00AS PPA (Asia Pacific) LNP* Verton* UV00AS is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3316 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | (DAM); ISO 1183 |
DSM Akulon® Ultraflow™ K-FHG12 Nylon 6-60% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
Eurostar Starflam PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)Information provided by Eurostar. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
BASF Heligoen® Blue L 6901 F Color Additive Description: Very brilliant a-phthalocyanine blues with high color strength and excellent flocculation resistance (L 6905 F is more brilliant and stronger than L 6901F).Chemical Structure: Cu-phthal.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | Liquid |
3M Novec™ 7300 Engineered Fluid 3M™ Novec™ 7300 fluid is a clear, colorless, odorless fluid that has utility in a wide variety of applications, including heat transfer, lubricant deposition, electronic testing and cleaning appli.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | |
Polystrand ThermoPro™ IE7015X X-Ply Cross-Ply Polypropylene-Glass Composite 2-Ply with Fiber Orientation at 0° & 90°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary ther.. |
|||
Density | 1.66 g/cc | 0.0600 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp PK0069 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0069 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |