SABIC Innovative Plastics LNP Thermocomp JF008 PES

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp JF008 PES.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* JF008 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ASTM D 792
1.66 g/cc
0.0600 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 134 MPa
19400 psi
ISO 527
149 MPa
21600 psi
ASTM D 638
Elongation at Break 1.4 %
1.4 %
ISO 527
2.1 %
2.1 %
ASTM D 638
Flexural Strength 202 MPa
29300 psi
ISO 178
Flexural Modulus 11.9 GPa
1730 ksi
ISO 178
Izod Impact, Notched 0.960 J/cm

@Temperature 23.0 °C
1.80 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 6.19 J/cm

@Temperature 23.0 °C
11.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 8.00 kJ/m²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 31.0 kJ/m²

@Temperature 23.0 °C
14.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U