Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D1475 |
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive
(discontinued **) CX-943 is a one-component polyurethane-based squeegee-grade, structural adhesive. Its elastomeric properties enable it to move with substrates as it expands and contracts. The patented formula is .. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH
(dis AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Density | 1.26 - 1.42 g/cc | 0.0455 - 0.0513 lb/in³ | Average value: 1.37 g/cc Grade Count:43 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp DP003XXP PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DP003XXP is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features include: Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP UL002S PPA LNP* LUBRICOMP* UL002S is a compound based on Polyphthalamide resin containing 10% PTFE. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Stat-kon AE0039 ABS LNP STAT-KON* AE0039 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber, Flame Retardant. Added features of this material include: Electrically Conductive.This dat.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PC SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation pr.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Techmer ES HiFill® PEI HF BK Availability: North AmericaForms: PelletsFeatures: High FlowAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66 LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
ExxonMobil Exxtral™ MDK340 Performance Polyolefin Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Adell BJ-14 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
BASF 4-Chlorbutyryl Chloride Formula: C4H6Cl2OCAS: 4635-59-0Description: 4-Chlorobutyryl chloride is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: 4-Chlorobutanoic acid ch.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
BASF Elastollan® M80A55 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Unitika U-8000 U series resins are polymer alloys that are improved in resistance to oils and chemicals, the shortcoming of amorphous resins. They are transparent and have a greater moisture blocking property than.. |
|||
Density | 1.26 - 1.42 g/cc | 0.0455 - 0.0515 lb/in³ | Average value: 1.31 g/cc Grade Count:7 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | Geon® 1169; Internal Method |
PolyOne Syncure™ V0044G S-1 RoHS Natural Polyethylene, Crosslinked (XLPE) Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System.Information provided by PolyOne |