Material Notes:
Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistance. UL continuous service rating of 90°CAvailability: Asia Pacific and North America Features:Detergent ResistantFilledGood Thermal Aging ResistanceHigh FlowHigh Heat ResistanceHigh Stiffness Processing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.3 MPa
5120 psi
2.0 in/min; ASTM D638
Elongation at Yield 2.3 %
2.3 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 3630 MPa
526000 psi
0.5 in/min; ASTM D790A
3990 MPa
579000 psi
0.05 in/min; ASTM D790B
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256A
Izod Impact Unnotched 4.20 J

@Temperature -17.8 °C
3.10 ft-lb

@Temperature 0.000 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.8 °C
199 °F
ASTM D648