| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
| Water Absorption | 2.4 % | 2.4 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 40 | 40 | ASTM D785 |
| Tensile Strength, Ultimate | 29.0 MPa | 4210 psi | ASTM D638 |
| Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
| Elongation at Break | 51 % | 51 % | ASTM D638 |
| Flexural Yield Strength | 28.0 MPa | 4060 psi | ASTM D790 |
| Flexural Modulus | 0.0900 GPa | 13.1 ksi | ASTM D790 |
| Izod Impact, Notched | 3.26 J/cm | 6.11 ft-lb/in | ASTM D256 |
| 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 140 °C | 284 °F | Flow temperature, ASTM D569 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 175 °C | 347 °F | Center barrel temperature |