Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Nylene® 404 Nylon 6 Injection molding grade. Dry as molded. Nylene 404 is a heat stabilized version of 401 which is recommended for general purpose nylon molding applications in both thin and heavy sections. In additi.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Nylene® 600 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrif.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO.1183 DIN.53479 |
Omnia Plastica Omniamid PA 6 - Akulon 6 - at 50% RH Semi-crystalline polymer of polyamide obtained by the polymerisation of the caprolactam. Its large popularity is due to both its good overall features as well as its cost-performance relationship. T.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 RV0 9005 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, halogen and phosphorus free.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66 Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6 Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Gichem GIBLEND F70500 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, excellent mechanical and thermal properties, very high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Zytel® 103FHSA NC010 is a heat stabilized, lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 222 Black 1N PA66, Conditioned Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
Solvay TECHNYL® B 216 Natural D PA66/6, Conditioned Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183/A |
Solvay TECHNYL® C 206 PA6, Conditioned Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific) LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific) Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MF006AL PP LNP* THERMOCOMP* MF006AL is a compound based on Polypropylene resin containing 30% Glass Fiber. Characteristics of this grade are: Low Extractable. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide Nylon 66 with molybdenum disulfide, low friction and high abrasion resistance, for injection molding applications.Information provided by Polyram. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | DIN 53479 |
Polyram PlusTek PB702 Nylon 6, UV Stabilized Polyamide 6 UV stabilized for fast cycle injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | DIN 53479 |
Polyram PlusTek RB841 Nylon 6, Impact Modified Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | |
Covestro Texin® 945U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
DSM Akulon® S223-EH Nylon 66 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
E-Polymers TEKAMID® TA210F Fast Crystallinity PA66, DAM Fast crystallinityInformation provided by E-Polymers Co. Ltd. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | |
Arkema Group Orgalloy® LE 6000IH Nylon Alloy, Flexible Grade (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the covering of.. |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0339T30L Talc Reinforced |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | |
Epoxyset Epoxibond EB-177 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Density | 1.14 g/cc | 0.0412 lb/in³ | ASTM D792 |
PolyOne Lubri-Tech™ MP-000/15T Modified PPO - 15% PTFE
(discontinued **) Data provided by PolyOne. |