Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.17 - 1.50 g/cc | 0.0423 - 0.0542 lb/in³ | Average value: 1.28 g/cc Grade Count:46 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Density | 1.14 - 1.50 g/cc | 0.0412 - 0.0542 lb/in³ | Average value: 1.24 g/cc Grade Count:33 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Density | 1.35 - 1.50 g/cc | 0.0488 - 0.0542 lb/in³ | Compounded |
Polychloroprene Rubber (CR) Polychloroprene rubber usually withstands ozone, oli/fat/grease, and many solvents. It is impacted by esters, ketones, chlorinated solvents, aromatic hydrocarbons, strong oxidizing acids, and nitro.. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 320 Rigid PVC, Extrusion Lead Free Indoor profiles |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 325 Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock |
|||
Density | 1.40 - 1.50 g/cc | 0.0506 - 0.0542 lb/in³ | ISO 1183 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 1.00 - 1.50 g/cc | 0.0361 - 0.0542 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 821.084 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
Density | 1.30 - 1.50 g/cc | 0.0470 - 0.0542 lb/in³ | DIN 53479/A |
Stanelco Bioplast® Wrap 100 Biodegradable Plastic Bioplast Wrap 100 is a plasticiser-free thermoplastic material which allows the production of films with coated paper-like properties. Wrap 100 is an excellent, eco-friendly alternative to laminated.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.05 |
Sinotek Materials B Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
Sinotek Materials D Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 1.20 - 1.50 g/cc | 0.0434 - 0.0542 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America EM 7302LD-2 Long Glass Fiber Reinforced Epoxy EM 7302LD-2 is a long fiberglass reinforced epoxy molding compound with a low density inert filler. This compound is designed for applications where moderate strength and weight savings are desirabl.. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 0221/T Flexible PVC, Sheathing Lead Free Anti-roditor and termites (anti-UV) |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 73 Flexible PVC, Sheathing General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 90 Flexible PVC, Insulation Lead Free General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 75 Flexible PVC, Insulation General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 92/1 Flexible PVC, Insulation Power cables |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 0248/4 Flexible PVC, Flame Retardant Sheathing Hydrocarbon resistant sheathing |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1187 |
Fainplast Compounds GK 75 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 019/27 Halogen Free PVC Sheathing; high flexibility |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 039/31 Halogen Free PVC Sheathing, insulation; high flexibility |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 76/2 Flexible PVC, Sheathing General purposes |
|||
Density | 1.45 - 1.50 g/cc | 0.0524 - 0.0542 lb/in³ | |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.45 - 1.50 g/cc | 0.0524 - 0.0542 lb/in³ | |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 1.00 - 1.50 g/cc | 0.0361 - 0.0542 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 821.6 Zirconia-Yttria 80-20 (ZrO2-Y2O3) |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.06 |
Sinotek Materials C Graphite Sheet Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 0.700 - 1.50 g/cc | 0.0253 - 0.0542 lb/in³ | ± 0.07 |
Sinotek Materials D Graphite Roll Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g.. |
|||
Density | 1.46 - 1.50 g/cc | 0.0527 - 0.0542 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 28 Halogen Free PVC Sheathing; good mechanical properties |
|||
Density | 1.15 - 1.50 g/cc | 0.0415 - 0.0542 lb/in³ | Average value: 1.43 g/cc Grade Count:19 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |
|||
Density | 0.210 - 1.50 g/cc | 0.00759 - 0.0542 lb/in³ | Average value: 1.17 g/cc Grade Count:125 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |