Indoor profiles
Physical Properties Metric English Comments
Density 1.46 - 1.50 g/cc
0.0527 - 0.0542 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
ISO R 527
Tensile Strength, Yield 41.0 MPa
5950 psi
ISO R527
Elongation at Break 120 %
120 %
ISO R 527
Izod Impact, Unnotched 0.400 - 0.800 J/cm

@Temperature 23.0 °C
0.749 - 1.50 ft-lb/in

@Temperature 73.4 °F
ISO R180
Thermal Properties Metric English Comments
Vicat Softening Point 79.0 - 81.0 °C

@Load 5.00 kg
174 - 178 °F

@Load 11.0 lb
ISO R306