Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zhejiang Juner JEPPB003 High Glossy PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Zhejiang Juner New Materials Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zhejiang Juner JEPPB003 High Glossy PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electric Rice CookerInformation provided by Zhejiang Juner New Materials Co, Ltd.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
GB/1033
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
GB/15585
Melt Flow 15 g/10 min
15 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
GB/1040
Flexural Strength 45.0 MPa
6530 psi
GB/9341
Charpy Impact Unnotched NB
NB
IS0179-1:2000
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
IS0179-1:2000
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
GB1634
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
D257
Processing Properties Metric English Comments
Processing Temperature 160 - 250 °C
320 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 85.0 °C

@Time 10800 sec
185 °F

@Time 3.00 hour
Horizontal Oven
90.0 °C

@Time 7200 sec
194 °F

@Time 2.00 hour
Chute Hot-Wind
Injection Pressure 30.0 - 80.0 MPa
4350 - 11600 psi
Descriptive Properties Value Comments
Speed of Shoot, % 35-85