Westlake Tymax™ GT4157 Anhydride Modified Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Westlake Chemical Corporation
Trade Name Tymax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Tymax™ GT4157 Anhydride Modified Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake GT4157 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a coextruded tie layer in multilayer film applications. Westlake GT4157 is designed to tie LLDPE to resins that typically have poor bonding characteristics such as polyamide and EVOH. Its applications include: blown film, packaging, and tie-layer.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D4883
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
DSC; ASTM D3418
Crystallization Temperature 103 °C
217 °F
DSC; ASTM D3418