Material Notes:
Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoforming
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Modulus 1.52 GPa
220 ksi
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 97.0 µm/m-°C

@Temperature 20.0 °C
53.9 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL Recognized
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi