Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EDRO #2 Prehardened 4130 Holder Block

Category Metal , Ferrous Metal , Alloy Steel , AISI 4000 Series Steel , Chrome-moly Steel
Manufacturer EDRO
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EDRO #2 Prehardened 4130 Holder Block.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to indentation, and uniform hardness in all dimensions. Applications: holders/bolsters for plastic molds and die-casting dies, plastics and rubber molds with low requirements on polishability, support plates, and constructional partsInformation provided by EDRO
Mechanical Properties Metric English Comments
Hardness, Brinell 293 - 332
293 - 332
Hardness, Vickers 650

@Treatment Temp. 525 °C
650

@Treatment Temp. 977 °F
Nitriding in ammonia gas
700

@Treatment Temp. 570 °C
700

@Treatment Temp. 1060 °F
Tufftriding (Tenifer process)
Tensile Strength, Ultimate 793 MPa

@Temperature 399 °C
115000 psi

@Temperature 750 °F
Round bar 1" diameter, 310 HB
951 MPa

@Temperature 199 °C
138000 psi

@Temperature 390 °F
Round bar 1" diameter, 310 HB
1010 MPa

@Temperature 20.0 °C
146000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
Tensile Strength, Yield 627 MPa

@Temperature 399 °C
91000 psi

@Temperature 750 °F
Round bar 1" diameter, 310 HB
752 MPa

@Temperature 199 °C
109000 psi

@Temperature 390 °F
Round bar 1" diameter, 310 HB
800 MPa

@Temperature 20.0 °C
116000 psi

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
Elongation at Yield 18 %

@Temperature 20.0 °C
18 %

@Temperature 68.0 °F
in 2"
20 %

@Temperature 199 °C
20 %

@Temperature 390 °F
in 2"
23 %

@Temperature 399 °C
23 %

@Temperature 750 °F
in 2"
Reduction of Area 50 %

@Temperature 20.0 °C
50 %

@Temperature 68.0 °F
52 %

@Temperature 199 °C
52 %

@Temperature 390 °F
54 %

@Temperature 399 °C
54 %

@Temperature 750 °F
Charpy Impact 50.2 J

@Temperature 20.0 °C
37.0 ft-lb

@Temperature 68.0 °F
Round bar 1" diameter, 310 HB
55.6 J

@Temperature 199 °C
41.0 ft-lb

@Temperature 390 °F
Round bar 1" diameter, 310 HB
71.9 J

@Temperature 399 °C
53.0 ft-lb

@Temperature 750 °F
Round bar 1" diameter, 310 HB
Component Elements Properties Metric English Comments
Carbon, C 0.30 %
0.30 %
Chromium, Cr 1.0 %
1.0 %
Iron, Fe 96.72 %
96.72 %
As Balance
Manganese, Mn 1.1 %
1.1 %
Molybdenum, Mo 0.20 %
0.20 %
Silicon, Si 0.28 %
0.28 %
Sulfur, S 0.40 %
0.40 %
Descriptive Properties Value Comments
Color Code Blue
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved