LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer LyondellBasell (former Equistar)
Trade Name Microthene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsMicrothene MP564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. MP564189 is 16 mesh powder and is also available in pellet form Petrothene GA564189.Regulatory StatusMP564189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520.Processing TechniquesSpecific recommendations for processing MP564189 can only be made when the processing conditions, equipment and end use are known.
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Spiral Flow 32.0 cm
12.6 in
Equistar
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength at Break 8.27 MPa
1200 psi
20 in/min; ASTM D638
Tensile Strength, Yield 14.5 MPa
2100 psi
20 in/min; ASTM D638
Elongation at Yield 12 %
12 %
20 in/min; ASTM D638
1% Secant Modulus 434 MPa
63000 psi
0.5 in/min; ASTM D790
2% Secant Modulus 0.379 GPa
55.0 ksi
0.5 in/min; ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C
113 °F
ASTM D648
Vicat Softening Point 91.1 °C
196 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Compliance Properties Metric English Comments
FDA Yes
Yes
Processing Properties Metric English Comments
Rear Barrel Temperature 177 °C
350 °F
Middle Barrel Temperature 191 °C
375 °F
Front Barrel Temperature 204 °C
400 °F
Nozzle Temperature 204 °C
400 °F