Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1235x70 Cast Film Resin
(discontinued **) LL 1235x70 is a butene LLDPE with improved stiffness. It can be used alone or as a component in packaging and industrial film.Information provided by ExxonMobil Chemical |
|||
Melting Point | 122 °C | 252 °F | Exxon Method |
ExxonMobil Escorene® LL-5102 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL-5102 makes for effici.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Melting Point | 122 - 155 °C | 252 - 311 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Melting Point | 122 - 175 °C | 252 - 347 °F | |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Melting Point | 122 °C | 252 °F | DSC |
Silon Tabond 3045 Adhesive Resin TABOND 3045 is LLDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Str.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Melting Point | 122 °C | 252 °F | ISO 3146 |
Borealis Borcoat™ ME0420 Grafted Polyethylene Adhesive for Steel Pipe Coating Borcoat ME0420 is a maleic-anhydride grafted polyethylene polymer to be extruded on conventional LDPE extruders with flat die or crosshead and it has excellent adhesion to epoxy powder and the top c.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Borealis FG5223 Linear Low Density Polyethylene FG5223 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant and anti-block additives. This grade is developed for production of lamination film. FG5223 has good heat.. |
|||
Melting Point | 122 °C | 252 °F | ISO 11357-3 |
Borealis FG5224 Linear Low Density Polyethylene FG5224 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-block and medium slip additives. This grade is developed for production of lamination film. FG5224 .. |
|||
Melting Point | 122 °C | 252 °F | ASTM D3418 |
Westlake Tymax™ GA4402 Anhydride Modified Linear Low Density Polyethylene (Developmental Resin) Westlake GA4402 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Melting Point | 122 °C | 252 °F | DSC; ASTM D3418 |
Westlake Tymax™ GT4157 Anhydride Modified Linear Low Density Polyethylene Westlake GT4157 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Melting Point | 122 °C | 252 °F | Crystalline; ISO 11357 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Melting Point | 122 °C | 252 °F | Crystalline; ISO 11357 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Melting Point | 122 °C | 252 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5252.09 Compounding Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2045G Linear Low Density Polyethylene DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow DOWLEX™ 2071D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | Dow Method (DSC) |
Dow FLEXOMER™ ETS-9066 NT 7, 2mil Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an.. |
|||
Melting Point | 122 °C | 252 °F | ASTM D2117 |
Lushan M-10F Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melting Point | 122 °C | 252 °F | |
DuPont Fusabond® MX110D Linear Low Density Polyethylene
(discontinued **) Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic comp.. |
|||
Melting Point | 122 °C | 252 °F | |
DuPont Fusabond® MD226D Linear Low Density Polyethylene
(discontinued **) Typical Use: CompatibilizerCoupling agent for nonhalogen, flame retarded wire and cable compounds containing fillers such as aluminum trihydrate or magnesium hydroxideNatural fiber wood-plastic comp.. |