Westlake Plastics Radel® R 5500 Polyphenylsulfone

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Westlake Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Radel® R 5500 Polyphenylsulfone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress cracking resistance. These properties make Radel R stock shapes attractive for a variety of demanding applications. The standard color of Radel R is off white, but a transparent grade is available.Radel® is a trade name of Solvay Advanced Polymers. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 69.6 MPa
10100 psi
ASTM D638
Elongation at Break 60 - 120 %
60 - 120 %
ASTM D638
Elongation at Yield 7.2 %
7.2 %
ASTM D638
Tensile Modulus 2.34 GPa
340 ksi
ASTM D638
Flexural Yield Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Compressive Yield Strength 98.94 MPa
14350 psi
ASTM D695
Compressive Modulus 1.73 GPa
251 ksi
ASTM D695
Izod Impact, Notched 6.94 J/cm
13.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Tensile Impact Strength 399 kJ/m²
190 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear 55.8 µm/m-°C

@Temperature 20.0 °C
31.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.349 W/m-K
2.42 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 214 °C
417 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
405 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.787 mm
V-0

@Thickness 0.0310 in
Oxygen Index 38 %
38 %
ASTM D2863
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1746
Transmission, Visible 50 %
50 %
ASTM D1746
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+17 ohm-cm
>= 1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.45

@Frequency 1000 Hz
3.45

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 14.2 kV/mm
360 kV/in
ASTM D149
Dissipation Factor 0.00090

@Frequency 1000 Hz
0.00090

@Frequency 1000 Hz
ASTM D150