Polymer Property : Compressive Modulus = 251 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.73 - 2.59 GPa
251 - 375 ksi
Average value: 2.30 GPa Grade Count:3
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Compressive Modulus 1.73 GPa
251 ksi
ASTM D695
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Compressive Modulus 1.73 GPa
251 ksi
ASTM D695
Westlake Plastics Radel® R 5500 Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c..
Compressive Modulus 1.73 GPa
251 ksi
ASTM D695
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications
Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,..
Compressive Modulus 1.73 GPa
251 ksi
ASTM D695
Westlake Plastics Radel® R Polyphenylsulfone
Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr..