Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.73 - 2.59 GPa | 251 - 375 ksi | Average value: 2.30 GPa Grade Count:3 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Compressive Modulus | 1.73 GPa | 251 ksi | ASTM D695 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Compressive Modulus | 1.73 GPa | 251 ksi | ASTM D695 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Compressive Modulus | 1.73 GPa | 251 ksi | ASTM D695 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone For Medical Applications Medical grade Radel R5500 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Compressive Modulus | 1.73 GPa | 251 ksi | ASTM D695 |
Westlake Plastics Radel® R Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr.. |