Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wellman Wellpet® PR118-N2 Unfilled Polyester PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellpet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellpet® PR118-N2 Unfilled Polyester PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Unfilled Polyester PETInformation provided by Wellman.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527-93
Elongation at Break 600 %
600 %
ISO 527-93
Flexural Strength 70.0 MPa
10200 psi
ISO 178-93
Flexural Modulus 2.40 GPa
348 ksi
ISO 178-93
Izod Impact, Notched (ISO) 3.50 kJ/m²
1.67 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-93