Material Notes:
Description: High Impact Nylon 66Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183-87
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.016 - 0.020 cm/cm
0.016 - 0.020 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-93
Elongation at Break 80 %
80 %
ISO 527-93
Flexural Strength 50.0 MPa
7250 psi
ISO 178-93
Flexural Modulus 1.85 GPa
268 ksi
ISO 178-93
Izod Impact, Notched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-93