Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ NL-30CF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ NL-30GF/15T Black Polyamide 612 (Nylon 612) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
PolyOne LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Latishield 75/4-10A PBT, Steel Fiber Reinforced EMI shielding product based on Polybutylene Terephthalate (PBT). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu.. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP DX09410H PC LNP* LUBRICOMP* DX09410H is a compound based on Polycarbonate resin containing Proprietary FIllers. Added features of this grade include: Healthcare, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP SX93441D PA12 LNP* Lubricomp* SX93441D is a compound based on Nylon 12 containing Proprietary Fillers. Characteristics of this grade are: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm @Time 86400 sec |
0.0080 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm @Thickness 3.20 mm |
0.016 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm @Thickness 3.20 mm |
0.015 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm @Time 86400 sec |
0.010 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON FD000 PE LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0080 - 0.020 cm/cm | 0.0080 - 0.020 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T101 PET Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66 LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RF007ES PA 66 LNP* THERMOCOMP* RF007ES is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Heat Stabilized, Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66 LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.010 - 0.020 cm/cm @Time 86400 sec |
0.010 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | DIS 294-4 |
Wellman Wellamid® FR1841-BK1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | DIS 294-4 |
Wellman Wellamid® FR1841-N1 Nylon 66, Unfilled, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66 Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1482-WT1 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® XT1627-BK2 High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® MRB40K004-WT1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
LATI Later 4 PBT Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
Linear Mold Shrinkage, Transverse | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |