Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-A890 Aliphatic TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-A890 Aliphatic TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength 25.0 MPa
3630 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
100% Modulus 0.00600 GPa
0.870 ksi
ASTM D412
300% Modulus 0.0210 GPa
3.05 ksi
ASTM D412
Tear Strength 85.0 kN/m
485 pli
ASTM D624
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Processing Temperature 185 - 205 °C
365 - 401 °F
Copyright © lookpolymers.com All Rights Reserved