Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® TPU 85A 0152 S1

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® TPU 85A 0152 S1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength at Break 54.5 MPa
7900 psi
ASTM D638
Elongation at Break 560 %
560 %
ASTM D638
200% Modulus 0.00758 GPa
1.10 ksi
ASTM D412
Flexural Modulus 0.0862 GPa
12.5 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 72.8 °C
163 °F
ASTM D1525