Covestro Texin® 4210 Urethane Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Covestro
Trade Name Texin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® 4210 Urethane Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.0 MPa

@Strain 50.0 %
1740 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 131 µm/m-°C

@Temperature 20.0 °C
72.8 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
Vicat Softening Point 139 °C
282 °F
50°C/h 50N
Glass Transition Temp, Tg -35.0 °C
-31.0 °F
10°C/min
Processing Properties Metric English Comments
Melt Temperature 230 °C
446 °F
Injection Molding
Mold Temperature 30.0 °C
86.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi