Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Unipetrol PP MONSTEN® EB 501 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Unipetrol RPA
Trade Name PP MONSTEN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unipetrol PP MONSTEN® EB 501 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Made for extrusion applications. LHTA stabilization. Impact copolymer.Information provided by Unipetrol RPA
Physical Properties Metric English Comments
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ISO 527
Elongation at Break >= 200 %
>= 200 %
ISO 527
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Charpy Impact, Notched 0.850 J/cm²

@Temperature -20.0 °C
4.05 ft-lb/in²

@Temperature -4.00 °F
ISO 179
8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ISO 75
Vicat Softening Point 150 °C
302 °F
ISO 306
Copyright © lookpolymers.com All Rights Reserved