Tra-Con Tra-Bond RO7 Radio Opaque Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond RO7 Radio Opaque Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND RO-7 is a high viscosity epoxy resin system specifically developed for adhesive and coating applications where radio opacity is required. It can be used as an X-ray marker on in-vitro medical devices. This two-part black adhesive is easily mixed, used and cured at room temperature for bonding, lamination and repair applications by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND RO-7 provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants, and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 4.20 g/cc
4.20 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Black
Mix Ratio, parts by weight 100/11
Resin/Hardener