Tra-Con Tra-Bond 526M03 Fast Cure Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 526M03 Fast Cure Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 526M03 is a fast cure, high viscosity, two-component epoxy formulation. It develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. TRA-BOND 526M03 has good impact and thermal shock resistance, and yields excellent low stress, pot-and-polish connections which do not piston during cycle tests. It is also resistant to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 14500 cP
14500 cP
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 12.4 MPa
1800 psi
Lap shear, alum to alum, 15 min @ 120°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 125 °C
257 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 130 °C
0.117 hour

@Temperature 266 °F
15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
Pot Life 240 min
240 min
Descriptive Properties Value Comments
Color Golden
Hardener
Red Brown
Cured
Yellow
Resin