Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen EP640R Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP640R Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection molding of washing machine tub, thin-walled packaging, parts of electrical appliances, housewares. Moplen EP640R resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Optimized balance of stiffness and toughness; High impact strength even at low temperature; Low warpage and fast cycle time; High stiffnessApplications: Washing machine tub; Parts of electrical appliance; HousewaresInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm

@Temperature -20.0 °C
0.735 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.883 J/cm

@Temperature 23.0 °C
1.65 ft-lb/in

@Temperature 73.4 °F
ASTM D256