ExxonMobil Exxon Hyjet V

Category Fluid , Lubricant
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxon Hyjet V.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability means extent of fluid degradation in aircraft systems will be less than Type IV fluids, in-service fluid life will be longer, and aircraft operator maintenance costs will be lower. HyJet V provides excellent high and low temperature flow properties (kinematic viscosities) and rust protection. HyJet V has also demonstrated an improvement over the erosion protection performance afforded by Type IV fluids.Exxon HyJet V is designed for use in commercial aircraft phosphate ester hydraulic systems. It meets the SAE AS1241 requirements and is included in the Airbus NSA307110 and Boeing BMS 3-11M qualified products list. It is compatible in all proportions with commercial Type IV and Type V phosphate ester aviation hydraulic fluids.
Physical Properties Metric English Comments
Specific Gravity 0.998 g/cc
0.998 g/cc
25°C; ASTM D4052
Density 1.003 g/cc

@Temperature 15.6 °C
0.03624 lb/in³

@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 320
320
Index; ASTM D2270
Viscosity Measure 1400 cSt

@Temperature -54.0 °C
1400 cSt

@Temperature -65.2 °F
Kinematic Viscosity; ASTM D445
Kinematic Viscosity at 40°C (104°F) 10.8 cSt
10.8 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 3.6 cSt
3.6 cSt
ASTM D445
Evaporation Loss 15 %
15 %
6 hr @ 71°C
Mechanical Properties Metric English Comments
Bulk Modulus 1.448 GPa
210.0 ksi
Isothermal secant at 100°F/3000psi
Thermal Properties Metric English Comments
CTE, linear 860 µm/m-°C

@Temperature 25.0 - 100 °C
478 µin/in-°F

@Temperature 77.0 - 212 °F
Specific Heat Capacity 1.76 J/g-°C
0.420 BTU/lb-°F
Thermal Conductivity 0.138 W/m-K

@Temperature 40.0 °C
0.957 BTU-in/hr-ft²-°F

@Temperature 104 °F
Pour Point <= -62.0 °C
<= -79.6 °F
ASTM D97
Flammability Test 185
185
Fire Point [°C]
>= 427
>= 427
Auto Ignition [°C]
Flash Point 174 °C
345 °F
ASTM D92
Component Elements Properties Metric English Comments
Calcium, Ca 0.00070 %
0.00070 %
Chlorine, Cl <= 0.00080 %
<= 0.00080 %
H2O 0.10 %
0.10 %
Potassium, K 0.0038 %
0.0038 %
Sodium, Na 0.00050 %
0.00050 %
Sulfur, S 0.0050 %
0.0050 %
Electrical Properties Metric English Comments
Electrical Resistivity 250 ohm-cm

@Temperature 20.0 °C
250 ohm-cm

@Temperature 68.0 °F
Chemical Properties Metric English Comments
Total Acid Number 0.050
0.050
mgKOH/g; ASTM D974
Descriptive Properties Value Comments
Foam Sequence I, ASTM D1136 0/0
Foam Sequence II, ASTM D893 0/0
Foam Sequence III, ASTM D893 0/0
Particle Count, NAS 1638 Class 5
Sonic Shear Stability, KV change % 21
@ 40°C