Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 7.00 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 160 °C
0.117 hour

@Temperature 320 °F
Uniseal BETABRACE™ 85001 Epoxy
BETABRACE™ 85001 is a composite used for reinforcing sheet metal. It is composed of a moderate temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85001 provides ..
Cure Time 7.00 min

@Temperature 130 °C
0.117 hour

@Temperature 266 °F
Tra-Con Tra-Bond 526M03 Fast Cure Epoxy Adhesive
TRA-BOND 526M03 is a fast cure, high viscosity, two-component epoxy formulation. It develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that incl..
Cure Time 7.00 min

@Temperature 125 °C
0.117 hour

@Temperature 257 °F
Tra-Con Tra-Bond FS437 Low Viscosity High Impact Epoxy Adhesive
TRA-BOND FS437 is a two-part, low viscosity material formulated for optical applications which require excellent wicking, visible color and high strength. This material has been used successfully fo..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 155 °C
0.117 hour

@Temperature 311 °F
TC90
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 4.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
Cure Time 7.00 min

@Temperature 177 °C
0.117 hour

@Temperature 351 °F
3M Scotchcast™ 260 8 G Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to..
Copyright © lookpolymers.com All Rights Reserved