Material Notes:
TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation contains no solvents, and is easily mixed, handled and applied at room temperature as it has a very long useful pot-life, however a final elevated temperature bake is REQUIRED for complete cure. TRA-BOND 2208 develops rigid high-strength bonds with excellent mechanical, structural and electrical properties coupled with good color stability, moderate heat resistance and good shock resistance. It adheres to metals, glass, glass products and fabrics, ceramics, rigid plastics and other high-temperature resistant materials. Fully cured TRA-BOND 2208 has superior electrical properties, and it provides excellent resistance to water, weather, vapors, gases and petroleum fuels and lubricants, salt solutions, most mild acids and alkalis, and many other chemical compounds. An additional post-cure of 4 hours at 145°C is recommended when application temperatures higher than 145°C are anticipated.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 1030 cP

@Temperature 25.0 °C
1030 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Tensile Strength, Yield 60.0 MPa
8700 psi
Elongation at Yield 5.0 %
5.0 %
Izod Impact, Notched 0.155 J/cm
0.290 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+15 ohm-cm
2.30e+15 ohm-cm
1.40e+12 ohm-cm

@Temperature 150 °C
1.40e+12 ohm-cm

@Temperature 302 °F
Dielectric Constant 3.2

@Frequency 1000 Hz
3.2

@Frequency 1000 Hz
Dielectric Strength 15.6 kV/mm
395 kV/in
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
2 hrs @ 65°C + 4 hrs @ 130°C
600 min
10.0 hour
2 hrs @ 65°C + 8 hrs @ 115°C
Pot Life 7200 min
7200 min
(5 days)
Descriptive Properties Value Comments
Color Clear
Mix Ratio, parts by weight 100/3
Resin/Hardener