Michelman® VaporCoat® 1500

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name VaporCoat®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® VaporCoat® 1500.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Water, oil and moisture resistant product for paperUsage: VaporCoat® 1500 is a coating which provides excellent water, oil and grease resistance along with excellent MVTR properties.Application Data: VaporCoat® 1500 may be applied by either a rod or blade. When applied on 42 lb. (200 gsm) kraft paper using a 10 rod, this product typically demonstrates 15 minute Cobb values of
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
pH 9.0 - 10
9.0 - 10
Brookfield Viscosity 100 - 400 cP
100 - 400 cP
Spindle # 2, rpm 60
Viscosity Measurement 25 - 35
25 - 35
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance White to cream colored liquid
Solids Type Polymer