Material Notes:
TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete and many plastics exhibits medium shrinkage during cure and has good dimensional stability over a wide temperature range. Fully cured TRA-BOND 2162D is a tough, durable, high peel, semi-flexible electrically insulating adhesive with good low temperature mechanical, thermal shock and impact resistance properties. In addition, it provides good resistance to gases and vapors, weather, water, salt solutions, petroleum solvents and lubricants, gasoline, mild acids and alkalis, and other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
Mixed
Viscosity 54000 cP

@Temperature 25.0 °C
54000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Tensile Strength, Yield 6.89 MPa
1000 psi
Elongation at Yield 45 %
45 %
Izod Impact, Notched 2.19 J/cm
4.10 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.6

@Frequency 1000 Hz
4.6

@Frequency 1000 Hz
Dielectric Strength 14.2 kV/mm
360 kV/in
Dissipation Factor 0.10

@Frequency 1000 Hz
0.10

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 540 min
9.00 hour
6 hrs @ 25°C + 3 hrs @ 65°C
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Light Yellow
Mix Ratio, parts by weight 100/100
Resin/Hardener