Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 54000 cP

@Temperature 25.0 °C
54000 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 2162D Color Coded Smooth Paste Epoxy Adhesive
TRA-BOND 2162D epoxy system is color-coded for easy mixing and handling as a smooth paste, and it develops strong bonds to most materials including metals, glass, ceramics, leather, wood, concrete a..
Viscosity 54000 cP
54000 cP
uncured
Atom Adhesives AA-BOND F162 Epoxy Adhesive
AA-BOND F162 is a thixotropic electrical insulating epoxy adhesive system with low vapor pressure and outgassing characteristics. AA-BOND F162 was specifically developed for fiber optic, laser, phot..